Srečko Stopić (Avtor), Rebeka Rudolf (Avtor), Jelena Bogovic (Avtor), Peter Majerič (Avtor), Miodrag Čolić (Avtor), Sergej Tomić (Avtor), Monika Jenko (Avtor), Bernd Friedrich (Avtor)

Povzetek

Golden nanoparticles of different sizes and shapes (spherical, cylindrical, triangular and round) where prepared during a synthesis of gold with ultrasonic spray pyrolysis (USP) and hydrogen reduction. The experimental investigations of the (USP) method were performed with an ultrasonic source of 0.8 MHz and 2.5 MHz, acting on the water solution of HAuCl4 forming aerosols with micron-sized and nanosized droplets. The results of the investigation show that the final shape and size of the Au particles depend on the characteristics of the solution and the frequency of the ultrasound. The second step of synthesizing the Au nanoparticles includes the subsequent thermal decomposition of the aerosol droplets in a hydrogen atmosphere between 260°C and 500°C. The investigations showed that the Au nanoparticles prepared in this way are smaller and more homogeneous.

Ključne besede

gold;ultrasonic spray pyrolysis;reduction;nanoparticles;

Podatki

Jezik: Angleški jezik
Leto izida:
Tipologija: 1.01 - Izvirni znanstveni članek
Organizacija: IMT - Inštitut za kovinske materiale in tehnologije
Založnik: Inštitut za kovinske materiale in tehnologije Ljubljana
UDK: 669.21:620.3:66.017
COBISS: 17274390 Povezava se bo odprla v novem oknu
ISSN: 1580-2949
Št. ogledov: 1200
Št. prenosov: 68
Ocena: 0 (0 glasov)
Metapodatki: JSON JSON-RDF JSON-LD TURTLE N-TRIPLES XML RDFA MICRODATA DC-XML DC-RDF RDF

Ostali podatki

Sekundarni jezik: Slovenski jezik
Sekundarni naslov: Sinteza Au-nanodelcev, pripravljenih z ultrazvočno razpršilno pirolizo in redukcijo z vodikom
Sekundarni povzetek: Zlate nanodelce različnih velikosti in oblik (sferični, cilindrični, trikotni in okrogli) smo pripravili s sintezo zlata z uporabo ultrazvočne razpršilne pirolize (USP) in redukcije. Eksperimentalne raziskave USP-metode so bile izvedene z ultrazvočnim izvirom s frekvenco med 0,8 MHz in 2,5 MHz z delovanjem na vodno raztopino HAuCl4, kjer je prišlo do formiranja aerosolov z mikro- in nanovelikostjo kapljic. Rezultati preiskav kažejo, da je oblika in velikost nastalih Au-delcev odvisna od karakteristik raztopine in od frekvence ultrazvoka. Drugi proces sinteze Au-nanodelcev je vključeval kasnejšo toplotno dekompozicijo kapljic aerosola. Izveden je bil v vodikovi atmosferi med 260°C in 500°C. Preiskave so pokazale, da so tako izdelani Au-delci bolj homogeni in manjši.
Sekundarne ključne besede: zlato;ultrazvočna razpršilna piroliza;redukcija;nanodelci;
URN: URN:NBN:SI
Vrsta dela (COBISS): Znanstveno delo
Strani: str. 577-583
Letnik: ǂLetn. ǂ47
Zvezek: ǂšt. ǂ5
Čas izdaje: sep.-okt. 2013
ID: 9110781