Ervin Žveplan (Avtor), Aleš Straže (Avtor)

Povzetek

Raziskali smo akustične lastnosti bukovine (Fagus sylvatica L.) po hidrotermični obdelavi. Iz dveh bukovih hlodov smo izžagali 10 parov radialno orientiranih preizkušancev nominalnih dimenzij 500 mm % 160 mm % 12 mm ter jih naravno posušili. Preizkušance smo 1 uro tretirali v nadtlačnem hidrotermičnem procesu pri temperaturi 135 °C. Po uravnovešenju pri 20 °C in 50 % zračni vlažnosti smo preizkušancem določili gostoto, hitrost preleta ultrazvoka v posameznih anatomskih smereh ter barvo po CIELab sistemu. Pri impulznem prečnem mehanskem vzbujanju smo določili še kazalnike akustične kakovosti. Določili smo akustični koeficient (K), dušenje zvoka (tan ▫\delta$▫) in relativno učinkovitost akustične pretvorbe (RACE). Po hidrotermični obdelavi smo potrdili zmanjšanje gostote bukovine ter povečanje hitrosti zvoka in togosti v vseh anatomskih smereh. Mehanska anizotropija lesa se je po obdelavi zmanjšala. Celotne barvne spremembe so bile značilno linearno povezane s spremembo gostote in s tem ohranitvijo togosti bukovine. Kazalniki akustične kakovosti hidrotermično obdelane bukovine so se delno izboljšali. Potrdili smo višji specifični modul elastičnosti in akustični koeficient ter manjše dušenje prečnega nihanja hidrotermično obdelanega lesa

Ključne besede

les;bukev;Fagus sylvatica;hidrotermična obdelava;mehanske lastnosti;akustične lastnosti;

Podatki

Jezik: Slovenski jezik
Leto izida:
Tipologija: 1.01 - Izvirni znanstveni članek
Organizacija: UL BF - Biotehniška fakulteta
UDK: 630*812.12
COBISS: 2845577 Povezava se bo odprla v novem oknu
ISSN: 0024-1067
Št. ogledov: 921
Št. prenosov: 135
Ocena: 0 (0 glasov)
Metapodatki: JSON JSON-RDF JSON-LD TURTLE N-TRIPLES XML RDFA MICRODATA DC-XML DC-RDF RDF

Ostali podatki

Sekundarni jezik: Angleški jezik
Sekundarni naslov: Acoustic properties of beech wood after hydrothermal treatment
Sekundarni povzetek: We investigated the acoustic properties of beech wood (Fagus sylvatica L.) after hydrothermal treatment. Two beech logs were cut into 10 pairs of radially oriented specimens with the dimensions 500 mm % 160 mm % 12 mm and air dried. Specimens were thermally treated for 1 hour in saturated vapour pressure atmosphere at 135 °C. After the treatment the specimens were conditioned at 20 °C and 50 % RH and their wood density, speed of ultrasound in all directions and colour properties in CIELab colour space were determined. Free flexural vibration tests were used afterwards to determine the acoustic properties of wood. We defined acoustic coefficient (K), damping of sound (tan ▫\delta$▫) and relative acoustic conversion efficiency (RACE). The study confirmed a significant decrease of wood density after the hydrothermal processing. The increase in speed of ultrasound in hydrothermally-treated wood caused no change in the modulus of elasticity in all anatomical directions. Mechanical anisotropy of wood decreased slightly after the treatment. The colour measurements of specimens showed a linear correlation between the total colour change and change of wood density and stiffness. The acoustic properties of hydrothermally treated beech wood were partly improved due to the increase in the specific modulus of elasticity and the acoustic coefficient combined with the decrease in vibration damping
Sekundarne ključne besede: wood;beech;hydrothermal treatment;mechanical properties;acoustic characteristics;
Vrsta dela (COBISS): Članek v reviji
Strani: str. 5-14
Letnik: ǂLetn. ǂ66
Zvezek: ǂšt. ǂ2
Čas izdaje: 2017
DOI: 10.26614/les-wood.2017.v66n02a01
ID: 13763219
Priporočena dela:
, diplomsko delo
, diplomsko delo - visokošolski strokovni študij
, ni podatka o podnaslovu